current location:home > Product Center
Characteristics and Applications
The current efficiency is 20~26%, and the high deposition speed is 2~3 times that of traditional chrome plating; The coating crystallization is fine and bright, with a hardness of more than 900HV and a microcrack number of more than 400/cm.
It is used for electroplating hard chrome in construction machinery, automobiles, motorcycles and other fields.
| Chromic anhydride | 180~280 g/L |
| Sulfuric acid | 3~4.5 g/L |
| Trivalent chromium | 1.5~3 g/L |
| C-26 | 14~20 ml/L |